Nickel Alloy 200 Coil
SKU: HC-1146011233517436928
Nickel Alloy 200 coil is made of a pure nickel alloy with a chemical composition containing a minimum of 99% nickel. This alloy is the purest nickel alloy and is often chosen for use in extremely corrosive environments.

Key Features
- ✓Third-Party Inspection Support
- ✓Sufficient Inventory Supply
- ✓International Standard Certification
- ✓Custom Processing Service
Contact Us
- Phone:+86 15052357278
- Email:juniper@hongchen-steel.com
- WhatsApp:+86 15052357278
Scan to chat

Product Description
Nickel Alloy 200 coil is made of a pure nickel alloy with a chemical composition containing a minimum of 99% nickel. This alloy is the purest nickel alloy and is often chosen for use in extremely corrosive environments. Nickel 200 is a high-purity metal consisting primarily of nickel with a purity of 99.0%. Due to its excellent physical and chemical properties, it is widely used in various fields. Nickel alloy 200 coil has high corrosion resistance, can withstand corrosion from various acid and alkali liquids, and maintains stable performance at high temperatures. In addition, nickel 200 coil has good thermal and electrical conductivity and is an important electrical and thermal conductive material. This metal can be processed and heated through various processes to make products of different shapes and specifications. Lastly, Nickel 200 is a pure commercial nickel with extremely low carbon content that has been approved for use in high temperature environments up to 1230 ° C.
Product Parameters
| Product Name | Nickel Alloy 200 Coil |
| Thickness | 2.5mm-10.0 mm |
| Length | 2000mm,2440mm,3000mm,5800mm,6000mm,etc. |
| Width | 610-2000 mm |
| Standard | ASTM,AISI,JIS,GB,DIN,EN,etc. |
| Surface | BA,2B,NO.1,NO.4,4K,HL,8K,etc. |
| Certificate | ISO,SGS,BV |
| Production Technology | Hot Rolling,Cold Rolling |
Chemical Composition
| Gread | C | Si | S | Mn | Fe | Ni | Cu |
|---|---|---|---|---|---|---|---|
| Alloy 200 | 0.15 max | 0.35 max | 0.01 max | 0.35 max | 0.4 max | 99.0 min | 0.25 max |
Mechanical Properties
| Tensile Strength (ksi) | 0.2% Yield Strength (ksi) | Elongation% in 2 inches |
| 55 | 15 | 35 |
Physical Performance
| Units | Temperature in°C | |
| Density | 8.89 g/cm³ | Room |
| Specific Heat | 0.108 Kcal/kg.C | Room |
| Melting Range | 1435-1446°C | - |
| Modulus of Elasticity | 205 KN/mm² | Room |
| Electrical Resistivity | 9.6 µΩ.cm | 20° |
| Coefficient of Expansion | 13.3 µm/m °C | 20 - 100° |
| Thermal Conductivity | 70.3 w/m-° K | 20° |