Hastelloy B-3 Pipe
SKU: HC-1146012197104254976
Hastelloy B3 pipe performs better in terms of strength and corrosion resistance at high temperatures compared with traditional Hastelloy. B3 alloy has excellent stability and durability, especially in oxidizing and reducing environments, as well as extreme corrosive environments such as strong acid and strong alkali.

Key Features
- ✓Third-Party Inspection Support
- ✓Sufficient Inventory Supply
- ✓International Standard Certification
- ✓Custom Processing Service
Contact Us
- Phone:+86 15052357278
- Email:juniper@hongchen-steel.com
- WhatsApp:+86 15052357278
Scan to chat

Product Description
Hastelloy B3 pipe performs better in terms of strength and corrosion resistance at high temperatures compared with traditional Hastelloy. B3 alloy has excellent stability and durability, especially in oxidizing and reducing environments, as well as extreme corrosive environments such as strong acid and strong alkali. Hastelloy B3 is a nickel-based high-temperature alloy mainly consisting of nickel, molybdenum, cobalt and other elements, of which the nickel content is about 65%. This alloy material is optimized on the basis of Hastelloy B2. By improving the thermal stability of the material, it significantly enhances the corrosion resistance, while also effectively improving the hot forming and cold forming performance. In recent years, Hastelloy B3 pipe has been increasingly used in the production and manufacturing of chemical equipment. Hastelloy B3 material has many unique properties. Its high elongation provides favorable conditions for cold forming operations. Compared to austenitic stainless steel, Hastelloy B3 material is harder and therefore needs greater pressure during cold forming or step forming processes.
Product Parameters
| Product Name | Hastelloy B-3 Pipe | |
| Outer Diameter | Round Pipe | 4mm-200mm |
| Square Pipe | 10*10mm-100*100mm | |
| Rectangular Pipe | 10*20mm-50*100mm | |
| Wall Thickness | 0.6mm-6.0mm | |
| Length | 1-6 meters,Length can be customized | |
| Standard | ASTM,AISI,JIS,GB,DIN,EN,etc. | |
| Surface | Black,Bright Polished,Rough Turning,Matt Surface Treatment,No.4,BA,etc. | |
| Certificate | ISO,SGS,BV | |
| Production Technology | Hot Rolling,Cold Rolling | |
Chemical Composition
| C | Al | Si | P | S | Ti | V | Cr | Mn | Fe | Co | Ni | Cu | Zr | Nb | Mo | Ta | W | Not MO |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| 0.01 max | 0.5 max | 0.10 max | 0.03 max | 0.01 max | 0.2 max | 0.2 max | 1.0 - 3.0 | 3.0 max | 1.0 - 3.0 | 3.0 max | 65.0 min | 0.2 max | 0.1 max | 0.2 max | 27.0 - 32.0 | 0.2 max | 3.0 max | 94.0 - 98.0 |
Mechanical Properties
| Tensile Strength (ksi) | 0.2% Yield Strength (ksi) | Elongation% in 2 inches |
| 110 | 51 | 40 |
Physical Performance
| Units | Temperature in°C | |
| Density | 9.22 g/cm³ | Room |
| Specific Heat | 0.089 Kcal/kg.C | Room |
| Melting Range | 1370-1418°C | - |
| Modulus of Elasticity | 216 KN/mm² | Room |
| Electrical Resistivity | 137 µΩ.cm | Room |
| Coefficient of Expansion | 10.6 µm/m °C | 25 - 100° |
| Thermal Conductivity | 11.2 w/m-° K | Room |