蒙乃尔400卷
型号: HC-1146006177304936448
它是一种镍铜合金(约67%的镍–23%的铜),在高温下耐海水和蒸汽,以及耐盐和腐蚀性溶液。蒙乃尔合金400是必须通过冷加工硬化的固溶体合金。这些镍合金具有良好的耐腐蚀性、良好的焊接性和高强度等特性。

核心优势
- ✓支持三方检测
- ✓充足库存供应
- ✓国际标准认证
- ✓定制加工服务
联系我们
- 电话:+86 15052357278
- 邮箱:juniper@hongchen-steel.com
- WhatsApp:+86 15052357278
扫码沟通

产品描述
它是一种镍铜合金(约67%的镍–23%的铜),在高温下耐海水和蒸汽,以及耐盐和腐蚀性溶液。蒙乃尔合金400是必须通过冷加工硬化的固溶体合金。这些镍合金具有良好的耐腐蚀性、良好的焊接性和高强度等特性。
Product Parameters
| Product Name | Monel 400 Coil |
| Thickness | 2.5mm-10.0 mm |
| Length | 2000mm,2440mm,3000mm,5800mm,6000mm,etc. |
| Width | 610-2000 mm |
| Standard | ASTM,AISI,JIS,GB,DIN,EN,etc. |
| Surface | BA,2B,NO.1,NO.4,4K,HL,8K,etc. |
| Certificate | ISO,SGS,BV |
| Production Technology | Hot Rolling,Cold Rolling |
Chemical Composition
| Nickel,min A | Copper | lron,max | Manganese,max | Carbon,max | Silicon,max | Sulfur,max |
|---|---|---|---|---|---|---|
| 63.0% | 28.0% - 34.0% | 2.5% | 2.0% | 0.3% | 0.5% | 0.024% |
Mechanical Properties
| Condition (Temper) | Tensile Strength,min,psi (MPa) | Yield Strength A (0.2 % offset),min,psi (MPa) | Elongation in 2 in. or 50 mm,or 4D,min,% | Rockwell Hardness (B Scale) b,c |
|---|---|---|---|---|
| Hot-Rolled Plate | ||||
| Annealed | 70000 (485) | 28000 (195) | 35 | - |
| As-Rolled D,E | 75000 (515) | 40000 (275) | 25 | - |
| Hot-Rolled Sheet | ||||
| Annealed | 70000 (485) | 28000 (195) | 35 | - |
| Cold-Rolled Sheet | ||||
| Annealed | 70000 - 85000 (485 - 585) | 28000 (195) | 35 | - |
| Quarter-Hard | - | - | - | 73 - 83 |
| Half-Hard | - | - | - | 82 - 90 |
| Hard | 100000 (690) | 90000 (620) | 2 | - |
| Cold-Rolled Strip | ||||
| Annealed | 70000 - 85000 (485 - 585) F | 28000 (195) | 35 F | - |
| Skin Hard | - | - | - | 68 - 73 |
| Quarter-Hard | - | - | - | 73 - 83 |
| Half-Hard | - | - | - | 82 - 90 |
| Three-Quarter-Hard | - | - | - | 89 - 94 |
| Hard | 100000 (690) F | 90000 (620) F | 2 F | - |
| Spring Temper | - | - | - | 98 min |
Physical Performance
| Units | Temperature in°C | |
| Density | 8.14 g/cm³ | Room |
| Specific Heat | 0.105 Kcal/kg.C | Room |
| Melting Range | 1370-1400°C | - |
| Modulus of Elasticity | 196 KN/mm² | 20° |
| Electrical Resistivity | 113 µΩ.cm | 25° |
| Coefficient of Expansion | 14.1 µm/m °C | 25 - 100° |
| Thermal Conductivity | 11.1 w/m-° K | 25° |